Guide

Candle sinkholes: why holes form around the wick and how to fix them

Last reviewed November 19, 2026

A homemade candle can sink in the middle as its wax contracts while cooling. The outside sets first and the warmer center continues shrinking, leaving a dip or a hidden cavity near the wick. The repair depends on how deep it is. A shallow surface dip can be smoothed with low heat; a deeper cavity may need relief holes and a second pour of the same recipe.

Find the repair steps · See a supplier’s second-pour example · Download a batch record

What causes candle sinkholes

CauseWhy it leaves a hole
Wax shrinking as it coolsVillage Craft & Candle explains that the edges and the area around the wick harden first, and the warm centre keeps shrinking after that. The more it shrinks, the bigger the sinkhole.
A hard waxHarder waxes shrink more. Village Craft & Candle says beeswax shrinks by up to 10% from liquid to solid, and that hard pillar paraffins shrink enough to leave a sinkhole around the wick that needs a second pour. CandleScience calls deep sinkholes in pillars "very common", especially with paraffin.
Cooling too fastPutting candles in the fridge, near a fan or in cold air sets the outside before the inside, which traps air and deepens the hollow.
Cold jars, molds or work surfacesCold glass, metal molds and stone countertops chill the wax at the edges first.
Pouring too hotVillage Craft & Candle calls temperature the main culprit. Even soft container waxes can form small surface sinkholes when poured well above their recommended temperature.
Trapped airMakesy describes the holes as air trapped inside the candle. If the surface sets before bubbles rise out, they stay as cavities underneath.

Check for hidden air pockets

A smooth top doesn't always mean a solid candle. Air bubbles that couldn't escape can sit just under the surface beside the wick, and the burning candle will reach them later. On pillars and harder waxes, look for a slight dip or a dimple around the wick once the candle has set. If you see one, poke relief holes before you finish the top (step 2 below), rather than just melting the surface smooth. Northwood Candle notes that melting the top with a heat gun can itself leave a sinkhole as the new surface cools, so a deeper problem usually needs a second pour.

How to fix a candle with sinkholes

  1. Small dips in soft wax: use a heat gun. CandleScience suggests setting a heat gun to low, holding it fairly close and gently melting the surface. Village Craft & Candle adds that a hair dryer works too: heat the top evenly until the dips fill and the surface is level, without scorching the wick.
  2. Deeper holes: poke relief holes. Once the candle has partly set, poke a few holes around the wick with a skewer to break into any air pockets. Village Craft & Candle and Makesy both recommend this, so trapped air can escape and the next pour can fill the gaps.
  3. Top up with a second pour. Keep some wax back from the batch, with the same fragrance and dye, so the top matches. Remelt it and pour a thin layer once the candle has hardened. CandleScience's pillar tutorial heats the second pour 5°F (about 3°C) above the first pour temperature and fills only up to the level of the cooled wax. Northwood Candle suggests about 150 to 160°F (66–71°C) for repouring a container candle: too hot can remelt the candle, and too cool may not bond and can leave a visible line.
  4. Trim the wick afterwards. Northwood Candle advises waiting until the second layer has cooled before trimming, since the new layer changes the wick's height.

A second-pour temperature example

CandleScience’s pillar tutorial uses a first pour at 170°F (76.7°C), then a second pour at 175°F (79.4°C). That is a rise of 5°F, or 2.8°C. It is the process for that tutorial’s wax. Use your own product instructions to choose a repour temperature.

Keep wax type, oil load and dye consistent between the layers. Check the product temperature table and record both pours on the batch sheet.

How to prevent sinkholes next batch

  • Pour at your wax's temperature. Pour temperatures differ widely between waxes. Use the figure on your wax's data sheet, or see the candle wax temperature chart, and let the wax cool to it in the pour pot.
  • Warm the jars or molds. Village Craft & Candle suggests bringing containers to room temperature, or warming cold ones on a baking sheet in the oven at its lowest setting for 15 to 20 minutes. A heat gun also works.
  • Keep the room steady. Village Craft & Candle suggests a pouring room at about 70°F (21°C), ventilated but without drafts.
  • Cool slowly, at room temperature. Never speed up cooling in the fridge or near a fan. Set candles on a cooling rack about 4 inches (10 cm) apart, not on a cold countertop.
  • Plan for a second pour with hard waxes. With pillar paraffin or beeswax, assume you'll top up. Pour to the shoulder of the jar or mold first and save some wax for the second layer.

Change one thing at a time and write it down. The free candle recipe sheet has lines for pour temperature, room temperature and notes on the finished top.

Sinkholes, wet spots or tunneling?

What you seeWhen it appearsGuide
A dip or hole around the wickAs the candle cools after pouringThis page
Patches where wax has pulled from the glassAs the candle cools or later in storageWet spots
A hole burning straight down the middleWhile the candle is burningTunneling
Oily beads on the surfaceAfter curing or in storageSweating

Frequently asked questions

Why does my candle have a hole around the wick?

The wax shrank as it cooled. The edges and surface set first, and the warm wax in the centre kept shrinking afterwards, pulling down around the wick. Hard waxes, cooling too quickly, cold jars and pouring too hot all make it more likely.

How do you fix a sinkhole in a candle?

For a small dip, melt the surface level with a heat gun on low. For a deep hole, poke relief holes around the wick to open any air pockets, then pour a thin second layer of the same wax once the candle has hardened.

What temperature should a second pour be?

CandleScience's pillar tutorial uses 5°F (about 3°C) above the first pour temperature. For container candles, Northwood Candle suggests about 150 to 160°F (66–71°C). Too hot can remelt the candle underneath, and too cool may not bond.

Do soy candles get sinkholes?

Less often. Soft soy container wax shrinks only slightly, so it's more prone to wet spots than to sinkholes. A soy candle poured much hotter than recommended, or cooled too fast, can still form small surface dips.

Can I burn a candle with a sinkhole?

A shallow surface dip usually burns fine. A deep cavity near the wick is better fixed first with relief holes and a second pour, so the candle burns down through solid wax.

Save enough wax for the second pour. The wax & fragrance calculator estimates how much wax and fragrance oil your jar needs, so you can melt a little extra for topping up.

Sources: shrinkage mechanism, temperature, cooling, room and jar preparation, relief holes and heat gun or hair dryer fix from Village Craft & Candle: how to prevent and fix sinkholes; beeswax and paraffin shrinkage from Village Craft & Candle: why does candle wax shrink; second pour at 5°F above the first and pillar sinkholes from CandleScience: how to make a pillar candle; heat gun method from CandleScience support: fixing surface flaws; repour temperature, heat-gun sinkholes and wick trimming from Northwood Candle: how to repour candles; trapped air and relief holes from Makesy: how to fix common candle making issues.